| Appearance | blackish-brown oily liquid |
| Xylenol dithiophosphoric acid Content | 60% - 70% |
| Density (20°C) | 1.17 - 1.20 g/mL |
Exhibits strong collecting capability for lead, copper, and silver sulfide minerals, while also being effective for activated zinc sulfide ores. Through adsorption via hydrophobic groups, it enhances mineral surface hydrophobicity and promotes bubble-particle attachment, thereby increasing valuable component recovery.
Demonstrates pH-dependent behavior: shows weak pyrite collecting power in alkaline conditions, facilitating preferential flotation of lead and zinc minerals. Functions as a potent non-selective collector for most sulfide minerals in neutral to acidic environments.
The inherent frothing characteristics reduce dependency on additional frothing agents. In specific flotation setups, it helps establish appropriately sized and stable foam layers, improving separation efficiency. Under certain conditions, also exhibits auxiliary collecting effects for heavy metal oxide ores.
Efficient collection of lead, copper, silver, and activated zinc sulfide ores with versatile applicability.
Superior selectivity in alkaline media enables effective pyrite depression and target mineral separation.
Extended utility to oxide ore flotation under specific conditions, broadening application scope.